Property | Item No. | Unit | Value | |
1 | Density | g/cm3 | 0.94-0.96 | |
2 | average molecular weight | g/mol | 9.2X106 | |
3 | Tensile strength (23℃ in air) | MPa | 22 | |
4 | Breaking strength | MPa | 42 | |
5 | Tensile strain at break | % | 600 | |
6 | Charpy impact strength (notched) | mJ/mm2 | No break | |
7 | Ball indentation hardness | N/mm2 | 42 | |
8 | Shore D hardness | -- | D65 | |
9 | Abrading(sand slurry experiment) | -- | 100 | |
10 | Coefficient of Friction | -- | 0.09~0.1 |
1250X3130X(Thickness:1-300mm)、1250X4250X(Thickness:1-300mm) 1500X3000X(Thickness:1-300mm)、2030X8200X(Thickness:1-300mm)
Property | Item No. | Unit | Value | |
1 | Density | g/cm3 | 0.94-0.96 | |
2 | average molecular weight | g/mol | 9.2X106 | |
3 | Tensile strength (23℃ in air) | MPa | 22 | |
4 | Breaking strength | MPa | 42 | |
5 | Tensile strain at break | % | 600 | |
6 | Charpy impact strength (notched) | mJ/mm2 | No break | |
7 | Ball indentation hardness | N/mm2 | 42 | |
8 | Shore D hardness | -- | D65 | |
9 | Abrading(sand slurry experiment) | -- | 100 | |
10 | Coefficient of Friction | -- | 0.09~0.1 |